dc.description.abstractEn el presente informe se determina la correlación entre el índice de madurez de mezclas de concreto y su resistencia a la compresión, fabricadas con cemento portland tipo Ms y Ico. Se trabajó con un total de 84 probetas de relaciones agua cemento 0.54, 0.61 y 0.69, fabricadas y curadas en concordancia a la norma ASTM C 192. Con la ayuda de un equipo electrónico casero, calibrado bajo la norma ASTM C 1074. Se tomó las lecturas de la temperatura del concreto, a las edades de 1, 3, 7, 14, 21 y 28 días. Determinando, a las mismas edades, la resistencia a la compresión aplicando la norma ASTM C 39. El índice de madurez se procesó, en concordancia a la norma ASTM C1074, mediante la ecuación de Nurse-Saúl. Las ecuaciones y grados de correlación para el concreto con cemento Portland tipo MS: Relación a/c de 0.54: f´c = 49.885 ln (IM) – 229.84 y R2= 0.9479 Kg/Cm2 Relación a/c de 0.61: f´c = 41.537 ln (IM) – 188.57 y R2= 0.9476 Kg/Cm2 Relación a/c de 0.69: f´c = 32.558 ln (IM) – 145.42 y R2= 0.9514 Kg/Cm2 Para el concreto con Cemento Portland tipo Ico: Relación a/c de 0.54: f´c = 51.149 ln (IM) – 234.60 y R2= 0.9434 Kg/Cm2 Relación a/c de 0.61: f´c = 43.745 ln (IM) – 198.73 y R2= 0.9456 Kg/Cm2 Relación a/c de 0.69: f´c = 34.628 ln (IM) – 155.92 y R2= 0.9438 Kg/Cm2es_PE
dc.description.abstractIn this report the correlation between the index of maturity of concrete mixes and its compressive strength, made with portland cement type Ms and Ico is determined. We worked with a total of 84 samples of water cement ratios 0.54, 0.61 and 0.69, manufactured and cured in accordance with ASTM C 192 standard. With the help of a home electronic equipment, calibrated under standard ASTM C 1074. readings concrete temperature, at ages 1, 3, 7, 14, 21 and 28 days it was noted. Determining, at the same ages, the compressive strength using the ASTM F 39 standard. The maturity index is processed, according to the ASTM C1074 standard, using the equation of Nurse-Saul. Equations and degrees of correlation for Portland cement concrete with Ms: W / c ratio of 0.54: f’c = 49.885 ln (IM) - 229.84 and R2 = 0.9479 Kg/Cm2 W / c ratio of 0.61: f’c = 41.537 ln (IM) - 188.57 and R2 = 0.9476 Kg/Cm2 W / c ratio of 0.69: f’c = 32.558 ln (IM) - 145.42 and R2 = 0.9514 Kg/Cm2 For concrete with Portland cement type Ico: W / c ratio of 0.54: f’c = 51.149 ln (IM) - 234.60 and R2 = 0.9434 Kg/Cm2 W / c ratio of 0.61: f’c = 43.745 ln (IM) - 198.73 and R2 = 0.9456 Kg/Cm2 W / c ratio of 0.61: f’c = 34.628 ln (IM) - 155.92 and R2 = 0.9438 Kg/Cm2en_US
dc.description.uriTesises_PE
dc.formatapplication/pdfes_PE
dc.language.isospaes_PE
dc.publisherUniversidad Privada Antenor Orrego - UPAOes_PE
dc.rightsinfo:eu-repo/semantics/openAccesses_PE
dc.sourceUniversidad Privada Antenor Orregoes_PE
dc.sourceRepositorio Institucional - UPAOes_PE
dc.subjectÍndice de madurezes_PE
dc.subjectMezcla de concretoes_PE
dc.subjectResistencia de comprensiónes_PE
dc.titleCorrelación entre el índice de madurez de una mezcla de concreto y su resistencia a la compresiónes_PE
dc.typeinfo:eu-repo/semantics/bachelorThesises_PE
thesis.degree.levelTítulo Profesionales_PE
thesis.degree.grantorUniversidad Privada Antenor Orrego. Facultad de Ingenieríaes_PE
thesis.degree.nameIngeniero Civiles_PE
thesis.degree.disciplineIngeniería Civiles_PE


Ficheros en el ítem

Thumbnail

Este ítem aparece en la(s) siguiente(s) colección(es)

Mostrar el registro sencillo del ítem