dc.description.abstractLa presente tesis trata del análisis de las propiedades físico - mecánicas de un mortero fabricado con cemento TIPO ICo y adicionado con vidrio en polvo al 3%y 5%, que se utilizan en La Libertad para, para la utilización de un mortero de alta resistencia en morteros de mampostería y de impermeabilización que requieran de alta resistencia y para edificaciones de gran envergadura, al realizar la investigación sobre el mortero, nos enfocamos en determinar el nivel de confiabilidad del uso de los morteros en sus diferentes aplicaciones con la adición del vidrio en polvo, haciendo una comparativa de resultados, lo que concluirá como un proyecto experimental. Porque en este estudio someteremos a un grupo de objetos, que son nuestros testigos cúbicos de mortero y la pasta fresca con determinadas pruebas de laboratorio con el equipo de compresión, Deformimetro, aguja de vicat, maquina universal de carga, entre otros equipos de laboratorio. Se desarrolló el análisis de mediante la dosificación en relación cemento y arena 1:1.91 para una muestra de 800 g., y una relación agua cemento de a/c de 0.40 y 110 de agua, teniendo como un total de material de 910 g. La resistencia a compresión: Para los testigos evaluados hasta los 56 días los resultados fueron, para un diseño patrón de 41.03 MPa, para una adición de 3% de vidrio 41.03 MPa y para una adición de 5% de vidrio 37.76 MPa. La resistencia flexotracción: Para los testigos evaluados hasta los 56 días los resultados fueron, para un diseño patrón de 2.76 MPa, para una adición de 3% de vidrio 2.62 MPa y para una adición de 5% de vidrio 2.38 MPa. La resistencia retracción del mortero: Para los testigos evaluados hasta los 56 días los resultados fueron, para un diseño patrón de -0.92 mm/m, para una adición de 3% de vidrio -0.822mm/m y para una adición de 5% de vidrio -0.770 mm/m. El tiempo de fraguado del mortero: Al realizar este ensayo podemos analizar y corroborar que a mayor porcentaje de vidrio menor será la penetración a un diseño patrón 420 minutos, a un 3% de adición de vidrio el tiempo disminuya a 405 minutos y a un 5% entre 405 y 390 minutos, por las proporciones de absorción de agua que presenta cada diseño. Con esto concluimos que el vidrio mejora ciertas propiedades y que su adición en cantidades mayores puede ser perjudicial para los mismos.es_PE
dc.description.abstractThis thesis deals with the analysis of the physical - mechanical properties of a mortar made of cement TYPE ICo and added with 3% and 5% glass powder, which is used in La Libertad for the use of a high strength mortar in masonry and waterproofing mortars that require high strength and for largescale buildings, when conducting research on the mortar, we focus on determining the level of reliability of the use of mortars in their different applications with the frequency of powdered glass , comparing results, which will conclude as an experimental project. Because in this study we will submit a group of objects, which are our cubic witnesses of mortar and fresh paste with laboratory tests with the compression equipment, Deformimeter, vicat needle, universal loading machine, among other laboratory equipment. Consider the analysis of by dosing in cement and sand ratio 1: 1.91 for a sample of 800 g., and a cement water ratio of a / c of 0.40 and 110 of water, having as a total material of 910 g. The compressive strength: For the witnesses evaluated up to 56 days the results were, for a standard design of 41.03 MPa, for an addition of 3% glass 41.03 MPa and for an additional 5% of glass 37.76 MPa. Flexural strength: For the witnesses evaluated up to 56 days the results were, for a standard design of 2.76 MPa, for an addition of 3% glass 2.62 MPa and for an addition of 5% glass 2.38 MPa. The shrinkage resistance of the mortar: For the witnesses evaluated up to 56 days the results were, for a standard design of -0.92 mm / m, for an addition of 3% glass -0.822mm / mi for an addition of 5% glass -0.770 mm / m. Mortar setting time: By performing this test we can analyze and corroborate a higher percentage of glass, the lower the penetration to a standard design 420 minutes, a 3% glass addition time decreased to 405 minutes and 5% between 405 and 390 minutes, for the proportions of water absorption that each design presents. With this we conclude that glass improves the properties and additional characteristics that may be harmful to them.en_US
dc.description.uriTesises_PE
dc.formatapplication/pdfes_PE
dc.language.isospaes_PE
dc.publisherUniversidad Privada Antenor Orrego - UPAOes_PE
dc.relation.ispartofseriesT_ING.CIVIL_1803
dc.rightsinfo:eu-repo/semantics/closedAccesses_PE
dc.sourceUniversidad Privada Antenor Orregoes_PE
dc.sourceRepositorio Institucional - UPAOes_PE
dc.subjectCementoes_PE
dc.subjectMorteroes_PE
dc.titleAnálisis de las propiedades físico-mecánicas de un mortero fabricado con cemento tipo Ico y adicionado con vidrio en polvo al 3% y 5%es_PE
dc.typeinfo:eu-repo/semantics/bachelorThesises_PE
thesis.degree.levelTítulo Profesionales_PE
thesis.degree.grantorUniversidad Privada Antenor Orrego. Facultad de Ingenieríaes_PE
thesis.degree.nameIngeniero Civiles_PE
thesis.degree.disciplineIngeniería Civiles_PE


Ficheros en el ítem

Thumbnail

Este ítem aparece en la(s) siguiente(s) colección(es)

Mostrar el registro sencillo del ítem