dc.description.abstractLa siguiente investigación tuvo como propósito analizar la influencia de uso de vidrio reciclado molido al 5% y 10% en la resistencia a la compresión de concreto 210 kg/cm2, con agregados de la cantera ""La soledad”. Las problemáticas a las que enfrentamos son que al momento de elaborar la mezcla para las obras existe un mal uso de los materiales, y muchas veces estos mismos son de mala calidad. Además, sabiendo que la creación de obras que usan mezcla de concreto afecta directamente al medio ambiente, se planteó evaluar el uso de uno de los desechos más contaminantes y menos aprovechados en cuanto a reciclaje, el vidrio, como un posible componente de la mezcla de un concreto 210 kg/cm2. Habiéndose realizado 3 muestras diferentes, todas con un diseño de mezcla para un concreto 210 kg/cm2. La muestra patrón, que no lleva nada de cambios en su dosificación; la muestra con 5%, en la que se reemplazó un 5% de vidrio reciclado molido con su porcentaje de agregado fino y finalmente la muestra con un reemplazo de 10% de vidrio reciclado molido. Luego de realizarse las probetas y ensayarlas se obtuvieron que en cuanto a la muestra patrón está dentro del margen de una resistencia optima de un concreto 210 kg/cm2, en cuanto a la segunda muestra y tercera muestra la resistencia a la compresión que obtuvimos disminuyo considerablemente en comparación con nuestra muestra patrón, Concluyendo así que el vidrio molido reciclado molido perjudica a la resistencia a la compresión de un concreto 210 kg/cm2 con agregados de la cantera “La soledad” sin embargo el uso del vidrio reciclado molido es una muy buena opción para generar una gran reducción en el impacto ambientales_PE
dc.description.abstractThe purpose of the following research was to analyze the influence of the use of ground recycled glass at 5% and 10% on the compressive strength of 210 kg/cm2 concrete, with aggregates from the ""La Soledad"" quarry. The problems we face are that when preparing the mixture for the works there is misuse of materials, and many times these are of poor quality. Furthermore, knowing that the creation of works that use a concrete mixture directly affects the environment, it was proposed to evaluate the use of one of the most polluting and least used waste in terms of recycling, glass, as a possible component of the mixture of a concrete 210 kg/cm2. Having made 3 different samples, all with a mix design for 210 kg/cm2 concrete. The standard sample, which does not have any changes in its dosage; the sample with 5%, in which 5% of ground recycled glass was replaced with its percentage of fine aggregate and finally the sample with a replacement of 10% of ground recycled glass. After making the specimens and testing them, it was obtained that as for the standard sample it is within the range of an optimal resistance of a concrete 210 kg/cm2, as for the second sample and third sample, the compression resistance that we obtained decreased considerably. Compared to our standard sample, Thus concluding that ground recycled ground glass harms the compressive strength of a 210 kg/cm2 concrete with aggregates from the “La Soledad” quarry. However, the use of ground recycled glass is a very good option to generate a large reduction in the environmental impactes_PE
dc.description.uriTesises_PE
dc.formatapplication/pdfes_PE
dc.language.isospaes_PE
dc.publisherUniversidad Privada Antenor Orregoes_PE
dc.relation.ispartofseriesT_CIVIL_2512
dc.rightsinfo:eu-repo/semantics/closedAccesses_PE
dc.rights.urihttps://creativecommons.org/licenses/by/4.0/es_PE
dc.subjectConcretoes_PE
dc.subjectvidrio molidoes_PE
dc.subjectresistencia a la compresiónes_PE
dc.titleInfluencia de uso de vidrio reciclado molido al 5% y 10% en la resistencia a la compresión de concreto 210 kg/cm2, con agregados de la cantera "La soledad"es_PE
dc.typeinfo:eu-repo/semantics/bachelorThesises_PE
thesis.degree.grantorUniversidad Privada Antenor Orrego. Facultad de Ingenieríaes_PE
thesis.degree.nameIngeniero Civiles_PE
thesis.degree.disciplineIngeniería Civiles_PE
dc.subject.ocdehttp://purl.org/pe-repo/ocde/ford#2.01.00es_PE
renati.advisor.orcidhttps://orcid.org/0000-0002-8611-8813es_PE
renati.author.dni70468424
renati.author.dni71768502
renati.advisor.dni26732593
renati.typehttp://purl.org/pe-repo/renati/type#tesises_PE
renati.levelhttp://purl.org/pe-repo/renati/level#tituloProfesionales_PE
renati.discipline732016es_PE
renati.jurorLópez Carranza, Atilio Rubén
renati.jurorGalicia Guarniz, William Conrad
renati.jurorRamirez Muñoz, Carlos Javier
dc.publisher.countryPEes_PE


Ficheros en el ítem

Thumbnail
Thumbnail
Thumbnail

Este ítem aparece en la(s) siguiente(s) colección(es)

Mostrar el registro sencillo del ítem

info:eu-repo/semantics/closedAccess
Excepto si se señala otra cosa, la licencia del ítem se describe como info:eu-repo/semantics/closedAccess