dc.description.abstract | Se ha determinado el diseño de la sustitución del concreto normal por el concreto
con cascote, en la propiedad mecánica del concreto utilizando cemento portland
tipo I.
Para lo cual; se tomaron dos diseños de mezclas con relación a/c (0.68) y con un
asentamiento de 3”.
Se elaboró y curo 25 probetas cilíndricas para cada relación a/c en concordancia a
la Norma ASTM C 192 y ASTM C 39. Así mismo se tomó en cuenta los resultados
de ensayos con las edades de 7, 14 y 28 días respectivamente.
Se realizó el diseño de mezcla para una resistencia a la compresión de f`c 140
kg/cm2; con diseño de mezclas con concreto normal y con concreto de cascote
producto de la demolición de vivienda en la zona de Trujillo, conservando la misma
relación a/c de 0.68 para ambos diseños; teniendo un valor constante en la cantidad
de agregados que se utilizó para el ensayo realizado, así mismo logró determinar
que para ambos diseños de mezclas con concreto normal y concreto de cascote en
la edad de 7 días (el concreto normal tiene un porcentaje de resistencia a la
compresión de 70% a comparación del concreto de cascote se obtuvo 78%), en la
edad de 14 días (el concreto normal tiene un porcentaje de resistencia a la
compresión de 85% a comparación del concreto de cascote se obtuvo 85%) y
finalmente a los 28 días de curado el concreto normal tiene un porcentaje de
resistencia a la compresión de 115% a comparación del concreto de cascote se
obtuvo 116%. Cabe recalcar que se observó que la Resistencia según las edades
antes mencionadas no perjudican a la Resistencia patrón que es de F`C 140
kg/cm2 | es_PE |
dc.description.abstract | The design of the replacement of normal concrete with concrete with rubble has
been determined, based on the mechanical property of the concrete using type I
Portland cement.
For which; Two mix designs were taken with w/c ratio (0.68) and with a slump of 3”.
25 cylindrical specimens were prepared and cured for each w/c ratio in accordance
with ASTM C 192 and ASTM C 39. These results in their tests are ages of 7, 14 and
28 days respectively.
The mix design was carried out for a compressive strength of f`c 140 kg/cm2; with
mixture design with normal concrete and with rubble concrete resulting from the
demolition of housing in the Trujillo area, maintaining the same w/c ratio of 0.68 for
both designs; having a constant value in the amount of aggregates that was used
for the test carried out, it was also possible to determine that for both mixture designs
with normal concrete and rubble concrete at the age of 7 days (normal concrete has
a compressive strength percentage of 70% compared to rubble concrete, 78% was
obtained), at the age of 14 days (normal concrete has a compressive strength
percentage of 85%, compared to rubble concrete, 85% was obtained) and finally
after 28 days of curing, normal concrete has a compressive strength percentage of
115%, compared to rubble concrete, 116% was obtained. It should be noted that it
was observed that the Resistance according to the aforementioned ages does not
harm the standard Resistance, which is F`C 140 kg/cm2 | es_PE |
dc.description.uri | Tesis | es_PE |
dc.format | application/pdf | es_PE |
dc.language.iso | spa | es_PE |
dc.publisher | Universidad Privada Antenor Orrego | es_PE |
dc.relation.ispartofseries | T_CIVIL_2579 | |
dc.rights | info:eu-repo/semantics/closedAccess | es_PE |
dc.rights.uri | https://creativecommons.org/licenses/by/4.0/ | es_PE |
dc.subject | Concreto | es_PE |
dc.subject | Diseño de Mezcla | es_PE |
dc.title | Diseño de concreto F`C 140 Kg/cm2 a base de concreto cascote con cemento Portland Tipo I - Trujillo | es_PE |
dc.type | info:eu-repo/semantics/bachelorThesis | es_PE |
thesis.degree.grantor | Universidad Privada Antenor Orrego. Facultad de Ingenieria | es_PE |
thesis.degree.name | Ingeniero Civil | es_PE |
thesis.degree.discipline | Ingenieria Civil | es_PE |
dc.subject.ocde | https://purl.org/pe-repo/ocde/ford#2.01.00 | es_PE |
renati.advisor.orcid | https://orcid.org/0000-0001-5207-4421 | es_PE |
renati.author.dni | 70062927 | |
renati.author.dni | 44188388 | |
renati.advisor.dni | 40534510 | |
renati.type | https://purl.org/pe-repo/renati/type#tesis | es_PE |
renati.level | https://purl.org/pe-repo/renati/level#tituloProfesional | es_PE |
renati.discipline | 732016 | es_PE |
renati.juror | Hurtado Zamora, Oswaldo | |
renati.juror | Velásquez Diaz, Gilberto Anaximandro | |
renati.juror | Perrigo Sarmiento, Felix Gilberto | |
dc.publisher.country | PE | es_PE |