dc.description.abstractEn la presente investigación se estudia los concretos de alta resistencia preparados con diferentes porcentajes de Nanosílice (GAlA NANOSILICE) (0.3%; 0.5%; 0.7%), en base a un concreto patrón (C.P) diseñada con un Superplastificante (viscocrete sc-50), en una dosis del 0.1% respecto al peso del cemento, el objetivo principal fue determinar en cuanto incrementa la resistencia mecánica a la compresión en diferentes dosis de Nanosílice adicionadas en base al Concreto Patrón. Para esto, se propuso diseñar mezclas de concreto según la metodología propuesta por el ACI 211.4 para las resistencias a la compresión de 420 y 600 kg/cm2, utilizando tres dosificaciones de aditivo nanosílice de 0.3%, 0.5% y 0.7% en peso de cemento para cada resistencia, y tomando en cuenta parámetros para los concretos con aditivo de 1 a 2 pulgadas según el ACI 211.4para los concretos patrón (sin aditivo), que sirvan para establecer propiedades del concreto como su trabajabilidad y consistencia. Después de tener las dosificaciones adecuadas, se procedió al preparado de cada una de estas, realizando los siguientes ensayos al concreto en estado fresco: asentamiento (Slump), temperatura, peso unitario volumétrico y porcentaje de aire; posteriormente se realizaron ensayos al concreto en estado endurecido: resistencia a la compresión a 3, 7 y 28 días de edad, como resultado del proceso de análisis de resistencia a la compresión se logró conocer la más óptima de aditivo Nanosílice la cual es de 0.5%. Para definir las dosificaciones de aditivo nanosílice y de Superplastificante se usó la recomendación del fabricante que establecía un rango de 0.5% a 3.0% y 0.5% a 1.8% respectivamente, las dosificaciones de los agregados se partieron según la metodología de diseño del comité ACI 211.4. Para 420 kgf/cm2 el contenido óptimo es 0.50% logrando resistencia de 448.10 kgf/cm2 Para 600 kgf/cm2 el contenido óptimo es 0.50% logrando resistencia de 637.60 kgf/cm2es_PE
dc.description.abstractIn the present investigation, high strength concretes prepared with different percentages of Nanosilicate (GAlA NANOSILICE) (0.3%, 0.5%, 0.7%) are studied, based on a concrete pattern (CP) designed with a Superplasticizer (viscocrete sc-50), in a dose of 0.1% with respect to the weight of the cement, the main objective was to determine as it increases the mechanical resistance to compression in different doses of Nanosilica added on the basis of the Standard Concrete. For this, it was proposed to design concrete mixtures according to the methodology proposed by the ACI 211.4 for the compressive strengths of 420 and 600 kg / cm2, using three dosages of nanosilicate additive of 0.3%, 0.5% and 0.7% by weight of cement for each resistance, and taking into account parameters for concrete with additive of 1 to 2 inches according to the ACI 211.4 for the concrete pattern (without additive), which serve to establish concrete properties such as its workability and consistency. After having the appropriate dosages, we proceeded to the preparation of each one of these, performing the following tests on the concrete in fresh state: settlement (Slump), temperature, volumetric unit weight and percentage of air; Subsequently tests were performed on concrete in hardened state: resistance to compression at 3, 7 and 28 days of age, as a result of the compression resistance analysis process it was possible to know the most optimal Nanosilice additive which is 0.5%. To define the dosages of nanosilica additive and superplasticizer, the manufacturer's recommendation was used, which established a range of 0.5% to 3.0% and 0.5% to 1.8% respectively, the dosages of the aggregates were split according to the design methodology of the ACI 211.4 committee. For 420 kgf / cm2 the optimum content is 0.80% achieving resistance of 448.10 kgf / cm2. For 600 kgf / cm2 the optimum content is 0.80% achieving resistance of 637.60 kgf / cm2.en_US
dc.description.uriTesises_PE
dc.formatapplication/pdfes_PE
dc.language.isospaes_PE
dc.publisherUniversidad Privada Antenor Orregoes_PE
dc.relation.ispartofseriesT_ING.CIVIL_1563
dc.rightsinfo:eu-repo/semantics/openAccesses_PE
dc.rights.urihttps://creativecommons.org/licenses/by/4.0/es_PE
dc.sourceUniversidad Privada Antenor Orregoes_PE
dc.sourceRepositorio Institucional - UPAOes_PE
dc.subjectDiseño de mezclaes_PE
dc.subjectConcreto de alta resistenciaes_PE
dc.subjectSika ViscoCrete SC-50es_PE
dc.subjectGAIAes_PE
dc.titleDiseño de mezcla para un concreto de alta resistencia adicionando Sika ViscoCrete SC-50 y GAIAes_PE
dc.typeinfo:eu-repo/semantics/bachelorThesises_PE
thesis.degree.levelTítulo Profesionales_PE
thesis.degree.grantorUniversidad Privada Antenor Orrego. Facultad de Ingenieríaes_PE
thesis.degree.nameIngeniero Civiles_PE
thesis.degree.disciplineIngeniería Civiles_PE
dc.subject.ocdehttps://purl.org/pe-repo/ocde/ford#2.01.00
renati.typehttps://purl.org/pe-repo/renati/type#tesis
renati.levelhttps://purl.org/pe-repo/renati/level#tituloProfesional
dc.publisher.countryPEes_PE


Ficheros en el ítem

Thumbnail

Este ítem aparece en la(s) siguiente(s) colección(es)

Mostrar el registro sencillo del ítem

info:eu-repo/semantics/openAccess
Excepto si se señala otra cosa, la licencia del ítem se describe como info:eu-repo/semantics/openAccess