dc.description.abstract | En la presente tesis se realizó una investigación respecto al análisis del
módulo de elasticidad dinámico de un concreto F´c 280 kg/cm2, y se agregaron
fibras de acero trefilado al 1.5%, 3.0% y 4.5%, marca Sika® Fiber CHO 80/60 NB,
para reforzar el hormigón, este tiene utilidades en losas de concreto tradicionales e
industriales, elementos de hormigón prefabricado, especialmente encolados para
con ello permitir su homogenización durante su mezcla, así evitaremos la
aglomeración de fibras individuales, estas nos suman ductilidad, tenacidad y una
alta capacidad de soporte en un vasto rango de aplicaciones.
Este estudio tiene como principal objetivo determinar la variación del módulo
de elasticidad dinámico para nuestro concreto, adicionando el aditivo mencionado
anteriormente, con lo cual pretendemos elaborar una comparativa con información
corroborada, entre ensayos destructivos y no destructivos; con ello aspiramos
encontrar respuestas mediante el análisis del módulo de elasticidad estático,
usando el compresómetro y hallar el módulo de elasticidad dinámico usando el
equipo de resonancia ultrasónico Pundit ® Lab.
En el procedimiento determinamos el módulo de elasticidad por medio del
análisis de las características de los agregados finos y gruesos, haciendo uso de la
Norma Técnica Peruana NTP 400.012.; seleccionamos el total de especímenes de
hormigón necesarias referenciándonos en la Norma ASTM C-192.; encontramos la
resistencia a la compresión empleando cemento Sol Portland Tipo I adicionando
las fibras de acero trefilado al 1.5%, 3.0% y 4.5%, según la norma ASTM C-31;
determinamos el módulo de elasticidad estático del concreto usando la norma
ASTM C-469, con el ensayo destructivo mediante el uso del compresómetro; así
como también encontramos el módulo de elasticidad dinámico del concreto
basándonos la norma ASTM C-597, con el ensayo no destructivo mediante el uso
del ultrasonido; luego evaluamos los resultados mediante tablas y gráficos
comparativos de los testigos a compresión y frecuencia de resonancia ultrasónico.
La metodología empleada haciendo una comparativa de resultados, lo que
concluirá como un proyecto básico y aplicado porque al principio se va a recopilar
10
información o investigar teorías para luego realizar los diseños, con el fin de lograr
obtener mejores resultados del módulo de elasticidad dinámico.
Por último, concluiremos con los gráficos comparativos que nos muestran el
valor del módulo de elasticidad a 7, 14 y 28 días en diferentes porcentajes de
adición para la trabajabilidad del diseño de mezcla de F´c 280 Kg/Cm2
. | es_PE |
dc.description.abstract | In the present thesis, an investigation was carried out regarding the analysis
of the dynamic modulus of elasticity of a concrete F'c 280 kg/cm2, and 1.5%, 3.0%
and 4. 5%, Sika® Fiber CHO 80/60 NB brand, to reinforce the concrete, this has
utilities in traditional and industrial concrete slabs, precast concrete elements,
specially glued to allow its homogenization during mixing, thus avoiding the
agglomeration of individual fibers, these add ductility, toughness and a high bearing
capacity in a wide range of applications.
The main objective of this study is to determine the variation of the dynamic
modulus of elasticity for our concrete, adding the additive mentioned above, with
which we intend to elaborate a comparison with corroborated information, between
destructive and non-destructive tests; with this we aspire to find answers through
the analysis of the static modulus of elasticity, using the compressometer and to find
the dynamic modulus of elasticity using the ultrasonic resonance equipment Pundit
® Lab.
In the procedure we determined the modulus of elasticity by analyzing the
characteristics of fine and coarse aggregates, using the Peruvian Technical
Standard NTP 400.012; we selected the total number of concrete specimens
needed, referring to the ASTM C-192 Standard; we found the compressive strength
using Sol Portland Type I cement with the addition of drawn steel fibers at 1.5%,
3.0% and 4. 5%, according to the ASTM C-31 standard; we determined the static
modulus of elasticity of concrete using the ASTM C-469 standard, with the
destructive test through the use of the compressometer; we also found the dynamic
modulus of elasticity of concrete based on the ASTM C-597 standard, with the non destructive test through the use of ultrasound; then we evaluated the results through
comparative tables and graphs of the compression cores and ultrasonic resonance
frequency.
The methodology used making a comparative of results, which will conclude
as a basic and applied project because at the beginning we will collect information
12
or investigate theories to then make the designs, in order to achieve better results
of the dynamic modulus of elasticity.
Finally, we will conclude with the comparative graphs that show us the value
of the modulus of elasticity at 7, 14 and 28 days in different percentages of addition
for the workability of the mix design of F'c 280 Kg/Cm2 | en_US |
dc.description.uri | Tesis | es_PE |
dc.format | application/pdf | es_PE |
dc.language.iso | spa | es_PE |
dc.publisher | Universidad Privada Antenor Orrego | es_PE |
dc.relation.ispartofseries | T_CIVIL_2042 | |
dc.rights | info:eu-repo/semantics/openAccess | es_PE |
dc.rights.uri | https://creativecommons.org/licenses/by/4.0/ | es_PE |
dc.source | Universidad Privada Antenor Orrego | es_PE |
dc.source | Repositorio Institucional - UPAO | es_PE |
dc.subject | Modulo de Elasticidad Dinámico | es_PE |
dc.subject | Fibras de Acero Trefilado Aditivo | es_PE |
dc.title | Análisis del módulo de elasticidad dinámico para concreto f´c 280 kg/cm2 adicionando fibras de acero trefilado al 1.5%, 3% y 4.5% | es_PE |
dc.type | info:eu-repo/semantics/bachelorThesis | es_PE |
thesis.degree.level | Título Profesional | es_PE |
thesis.degree.grantor | Universidad Privada Antenor Orrego. Facultad de Ingeniería | es_PE |
thesis.degree.name | Ingeniero Civil | es_PE |
thesis.degree.discipline | Ingeniería Civil | es_PE |
dc.subject.ocde | https://purl.org/pe-repo/ocde/ford#2.01.00 | es_PE |
renati.advisor.orcid | https://orcid.org/0000-0003-3357-2315 | es_PE |
renati.author.dni | 46471153 | |
renati.author.dni | 70333263 | |
renati.advisor.dni | 40284306 | |
renati.type | https://purl.org/pe-repo/renati/type#tesis | es_PE |
renati.level | https://purl.org/pe-repo/renati/level#tituloProfesional | es_PE |
renati.discipline | 732016 | es_PE |
renati.juror | Hurtado Zamora, Oswaldo | |
renati.juror | Galicia Guarniz, William Conrad | |
renati.juror | Luján Silva, Enrique Francisco | |
dc.publisher.country | PE | es_PE |