Mostrar el registro sencillo del ítem

dc.contributor.advisorCancino Rodas, César Leónidas
dc.contributor.authorElorreaga Paiba, Carlos Alejandro
dc.contributor.authorGonzález Sánchez, Orlando Domingo
dc.creatorElorreaga Paiba, Carlos Alejandro
dc.date.accessioned2018-07-06T16:53:13Z
dc.date.available2018-07-06T16:53:13Z
dc.date.issued2018
dc.identifier.urihttps://hdl.handle.net/20.500.12759/4169
dc.description.abstractEn el presente trabajo se determinó la influencia de las macro-fibras de polipropileno y la forma del agregado grueso en la tenacidad del concreto fabricado con cemento portland tipo GU. Se elaboraron en total 90 probetas, según las normas UNE 83504 y UNE 83502, con 0, 3, 4, 6 y 8 kg de fibra de polipropileno por metro cúbico de concreto. El concreto se dosificó con relaciones a/c de 0.43, 0.48 y 0.55, agregado grueso de forma angular e irregular, con un tamaño máximo nominal de ¾”. A dichas probetas se las sometió al ensayo de doble punzonamiento en concordancia a la norma UNE 83515. Concluyendo que para las mezclas de concreto con agregado grueso de forma irregular y de tamaño máximo nominal de ¾”, se observó un incremento de la tenacidad conforme fue aumentando la dosificación de fibras, pero no logró optimizar de manera definida la tenacidad en el concreto; y para las mezclas de concreto con agregado grueso de forma angular y de tamaño máximo nominal de ¾”, obtuvieron el mayor incremento de latenacidad para una dosificación de 4 kg/mix3, siendo estas 504.50 Joules para una relación a/c de 0.43, 440.04 Joules para una relación a/c de 0.48 y 417.20 Joules para una relacióna/c de 0.55es_PE
dc.description.abstractIn the present work, the influence of polypropylene macro-fibers and the shape of the coarse aggregate on the toughness of the concrete manufactured with portland type GU cement was determined. A total of 90 specimens were prepared, according to the UNE 83504 and UNE 83502 standards, with 0, 3, 4, 6 and 8 kg of polypropylene fiber per cubic meter of concrete. The concrete was dosed with a / c ratios of 0.43, 0.48 and 0.55, coarse aggregate of angular and irregular shape, with a maximum nominal size of ¾ ““. Said test tubes were subjected to the double punching test in accordance with the UNE 83515 standard. Concluding that for the mixtures of concrete with coarse aggregate of irregular shape and maximum nominal size of ¾ ““, an increase of the tenacity was observed as the dosage of fibers was increasing, but it did not manage to definitively optimize the tenacity in the concrete; and for concrete mixtures with coarse aggregate of angular shape and maximum nominal size of ¾ ““, they obtained the highest increase in toughness for a dosage of 4 kg / m3, these being 504.50 Joules for an a / c ratio of 0.43, 440.04 Joules for an a / c ratio of 0.48 and 417.20 Joules for an a / c ratio of 0.55.en_US
dc.description.uriTesises_PE
dc.formatapplication/pdfes_PE
dc.language.isospaes_PE
dc.publisherUniversidad Privada Antenor Orrego - UPAOes_PE
dc.relation.ispartofseriesT_ING.CIVIL_1537
dc.rightsinfo:eu-repo/semantics/openAccesses_PE
dc.sourceUniversidad Privada Antenor Orregoes_PE
dc.sourceRepositorio Institucional - UPAOes_PE
dc.subjectMacro fibrases_PE
dc.subjectPolipropilenoes_PE
dc.titleUso de macro-fibras de polipropileno y forma de agregado grueso en la tenacidad del concreto fabricado con cemento Portland tipo GUes_PE
dc.typeinfo:eu-repo/semantics/bachelorThesises_PE
thesis.degree.levelTítulo Profesionales_PE
thesis.degree.grantorUniversidad Privada Antenor Orrego. Facultad de Ingenieríaes_PE
thesis.degree.nameIngeniero Civiles_PE
thesis.degree.disciplineIngeniería Civiles_PE